Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.023 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.023 cm/cm

@Thickness 3.20 mm
0.023 in/in

@Thickness 0.126 in
Flow; DAM
DuPont Performance Polymers Zytel® FE4200 BK136 Nylon 66  (Unverified Data**)
Zytel® FE4200 BK136 is a low die deposit polyamide 66 extrusion resin.Information provided by DuPont Performance Polymers