Bulk Density 2.64 g/cc

@Temperature 1450 °C,
Time 7200 sec
0.0954 lb/in³

@Temperature 2640 °F,
Time 2.00 hour
Chosun Refractories AU3 Blast Furnace Runner Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).