Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.02 g/cc @Temperature 1000 °C, Time 10800 sec |
0.0730 lb/in³ @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories C40 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |