Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.80 g/cc @Temperature 800 °C |
0.0650 lb/in³ @Temperature 1470 °F |
|
Sharadaa Ceramics Sharada RFC-Fused Silica Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |