Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.10 g/cc @Temperature 1400 °C |
0.0759 lb/in³ @Temperature 2550 °F |
|
Sharadaa Ceramics Sharada RFC-45 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Bulk Density | 2.10 g/cc @Temperature 110 °C, Time 86400 sec |
0.0759 lb/in³ @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories RP-210 Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |