Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.059 cm/cm | 0.059 in/in | ISO Data |
BASF Ultramid® B3ZG7 OSI BK23273 35% Glass Filled PA6 (Dry) Ultramid B3ZG7 OSI BK23273 is a 35% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet demanding mechanical and chemical requi.. |