Polymer Property : Linear Mold Shrinkage, Transverse = 0.0392 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00300 - 0.0392 cm/cm
0.00300 - 0.0392 in/in
Average value: 0.0133 cm/cm Grade Count:37
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..