Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.031 cm/cm | 0.031 in/in | ISO 294-4 |
Azoty Tarnow™ TARNOFORM 500 UV POM High flow injection molding grade based on Tarnoform 500 modified with carbon black giving best weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |