Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.028 cm/cm | 0.028 in/in | |
Plastcom SLOVAMID 66 HI/1 TS PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Linear Mold Shrinkage, Transverse | 0.028 cm/cm | 0.028 in/in | |
Plastcom SLOVAMID 66/6 HI/1 PA66/6, improved strength FeaturesMix of polyamide 66/6 modified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets fo.. |
|||
Linear Mold Shrinkage, Transverse | 0.028 cm/cm @Time 86400 sec |
0.028 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Faradex KS003AI Acetal Copolymer (Europe-Africa-Middle East) LNP* FARADEX* KS003AI is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber. Added features include; EMI/RFI Shielding, Electrically Conductive.This data was supplied by SAB.. |
|||
Linear Mold Shrinkage, Transverse | 0.028 cm/cm | 0.028 in/in | ASTM D955 |
Shell Carilon® DP R1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1000 is a high flow developmental engineering polyketone resin from Shell Chemi.. |