Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0265 cm/cm | 0.0265 in/in | 60x60x4; ISO 294-4 |
Azoty Tarnow™ TARNOFORM 300 GF4 POM 20% glass fiber reinforced injection molding grade with very high strength.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |