Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0263 cm/cm
0.0263 in/in
Plastcom SLOVALEN PQ 83 N PP, imp. strength
FeaturesPP modified with natural caoutchouc. The addition of thermoplastic caoutchouc causes increased toughness. General application in all industry branches. Delivered in natural mode and in the f..
Linear Mold Shrinkage, Transverse 0.0263 cm/cm
0.0263 in/in
Plastcom SLOVALEN PQ 53 N PP, imp. strength
FeaturesPP modified with natural caoutchouc. The addition of thermoplastic caoutchouc causes increased toughness. General application in all industry branches. Delivered in natural mode and in the f..