Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0253 cm/cm | 0.0253 in/in | STN EN ISO 294-4 |
Plastcom PLASTAMID® 6 HI PA6 with improved impact strength PA 6 for injection molding, impacted, modified with thermoplastic elastomer, determined for high impacted moldings also at low temperature. Delivered in natural mode and in the full RAL color scale... |
|||
Linear Mold Shrinkage, Transverse | 0.0253 cm/cm | 0.0253 in/in | |
Plastcom SLOVAMID 6 LI PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |