Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0252 cm/cm | 0.0252 in/in | |
Plastcom SLOVALEN PC 71 T 15 PP, 15% mineral filling FeaturesModified PP for injection moulding with the content of 15% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches - pack.. |