Polymer Property : Linear Mold Shrinkage, Transverse = 0.0235 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0235 - 0.0275 cm/cm
0.0235 - 0.0275 in/in
LATI Latan 13E71 POM
Polyoxymethylene (POM). Toughened. Medium viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided ..
Linear Mold Shrinkage, Transverse 0.0235 - 0.0275 cm/cm
0.0235 - 0.0275 in/in
LATI Latan 3E71 POM
Polyoxymethylene (POM). Toughened. High viscosity. Good elongation and impact resistanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by ..