Polymer Property : Linear Mold Shrinkage, Transverse = 0.0215 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0120 - 0.0215 cm/cm
0.0120 - 0.0215 in/in
Average value: 0.0150 cm/cm Grade Count:7
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..