Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0207 cm/cm | 0.0207 in/in | |
Plastcom SLOVAMID 6 MI PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Linear Mold Shrinkage, Transverse | 0.0207 cm/cm | 0.0207 in/in | |
Solvay TECHNYL® C 236SI PA6, DRY Description: Unreinforced polyamide 6 with high impact strength for injection molding.Available in: Europe and North AmericaProduct Applications: TECHNYL® C 236SI has high impact strength and fle.. |
|||
Linear Mold Shrinkage, Transverse | 0.0207 cm/cm | 0.0207 in/in | |
Solvay TECHNYL® C 536XT PA6, DRY Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing.. |