Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0206 cm/cm
0.0206 in/in
Plastcom SLOVALEN PC 19 GF 20 PP, 20% glass fibre, mod. of mech. properties
FeaturesModified copolymer PP for iextrusion, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. Applied i..
Linear Mold Shrinkage, Transverse 0.0206 cm/cm
0.0206 in/in
Plastcom SLOVALEN PC 79 GF 20 PP, 20% glass fibre, mod. of mech. prop.
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...