Polymer Property : Linear Mold Shrinkage, Transverse = 0.0204 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0204 cm/cm
0.0204 in/in
STN 64 0808
Plastcom SLOVAMID 6 HI Polyamide 6, Impacted
FeaturesPA 6 with the content of thermoplastic elastomer. Impacted, for mouldings with high toughness either at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets..
Linear Mold Shrinkage, Transverse 0.0204 cm/cm
0.0204 in/in
Plastcom SLOVAMID 6 HI/1 TLS PA6, improved strength
FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme..
Linear Mold Shrinkage, Transverse 0.0204 cm/cm
0.0204 in/in
STN 64 0808
Plastcom SLOVAMID 6 LI/1 Polyamide 6, Impacted
FeaturesPA 6 with the content of thermoplastic elastomer. Impacted, for mouldings with high toughness either at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets..