Polymer Property : Linear Mold Shrinkage, Transverse = 0.0178 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0178 cm/cm
0.0178 in/in
Sheet
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT
Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic ..