Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0141 cm/cm | 0.0141 in/in | |
Plastcom SLOVAMID 6 GF 10 FRA 5 PA6, 10% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 10% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Linear Mold Shrinkage, Transverse | 0.0141 cm/cm | 0.0141 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 GF 45 Polyamide 6, 45% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Linear Mold Shrinkage, Transverse | 0.0141 cm/cm | 0.0141 in/in | |
Plastcom SLOVAMID 66 T 15 PA66, 15% mineral filling FeaturesPA 66 with the content of 15 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel.. |
|||
Linear Mold Shrinkage, Transverse | 0.0141 cm/cm | 0.0141 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 GF 15 FRA 5 Polyamide 6, 15% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |