Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0133 cm/cm | 0.0133 in/in | |
Plastcom SLOVASTER® B1 GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Linear Mold Shrinkage, Transverse | 0.0133 cm/cm | 0.0133 in/in | |
Plastcom SLOVASTER® B1 HML GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Linear Mold Shrinkage, Transverse | 0.0133 cm/cm | 0.0133 in/in | 150x105x3; 300°C / MT 80°C; 400 bar; ISO 2577 |
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0133 cm/cm | 0.0133 in/in | ISO 294-4 |
DSM EcoPaXX® Q-KGS6 PA410-GF30 FR 30% Glass Reinforced, Flame Retardant (Halogen free) |