Polymer Property : Linear Mold Shrinkage, Transverse = 0.0128 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00750 - 0.0128 cm/cm
0.00750 - 0.0128 in/in
Average value: 0.0113 cm/cm Grade Count:3
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..