Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0118 cm/cm | 0.0118 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 GF 25 Polyamide 66, 25% Glass Fiber FeaturesChemically reinforced with 25% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Linear Mold Shrinkage, Transverse | 0.0118 cm/cm | 0.0118 in/in | |
Plastcom SLOVAMID 66 GF 30 HI PA66, 30% glass fibre, improved strength FeaturesPA 66 for injection moulding, chemically strengthened with 30% glass fibre and with the content of thermoplastic kaoutchouc. Application: impacted mouldings and mouldings with high strength .. |