Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0103 cm/cm | 0.0103 in/in | STN EN ISO 294-4 |
Plastcom PLASTALEN® PQ 81 T 20 Polypropylene reinforced with mineral filler, impact modified Modified PP for injection molding with the content of 20% mineral filler. General application in all industry branches. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Linear Mold Shrinkage, Transverse | 0.0103 cm/cm | 0.0103 in/in | STN EN ISO 294-4 |
Plastcom PLASTALEN® T 20 Regranulate Polypropylene reinforced with mineral filler PP regranulate for injection molding with 20% mineral filler. Application for general purposes in all industrial sectors.Information Provided by Plastcom spol. s r.o. |
|||
Linear Mold Shrinkage, Transverse | 0.0103 cm/cm | 0.0103 in/in | |
Plastcom SLOVALEN PQ 81 T 20 PP, 20% mineral filling FeaturesModified PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Linear Mold Shrinkage, Transverse | 0.0103 cm/cm @Time 86400 sec |
0.0103 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized. |