Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0102 cm/cm | 0.0102 in/in | |
Plastcom SLOVALEN PH 56 T FRD 1 PP, flame retardant FeaturesModified homopolymer PP for injection moulding with decreased flammability. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil forms, guides, co.. |