Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00980 - 0.0271 cm/cm | 0.00980 - 0.0271 in/in | Average value: 0.0159 cm/cm Grade Count:14 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |