Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0084 cm/cm | 0.0084 in/in | |
Plastcom SLOVAMID 6 T 30 TS PA6, 30% mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application. Increased modulus in tension - strength of the material. PA matrix reduction. PA for injection moulding with the content.. |
|||
Linear Mold Shrinkage, Transverse | 0.0084 cm/cm | 0.0084 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 T 30 Polyamide 6, 30% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |