Polymer Property : Linear Mold Shrinkage, Transverse = 0.0026 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0026 cm/cm
0.0026 in/in
ISO 294-4, 2577
Lanxess Pocan® B 2505 000000 PBT
PBT, non-reinforced, injection molding, flame retardant
Linear Mold Shrinkage, Transverse 0.0026 cm/cm
0.0026 in/in
GB/T 15585-1995
Sichuan Deyang Haton® hCF31 Polyphenylene Sulfide
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD