Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0016 cm/cm | 0.0016 in/in | ISO 294-4, 2577 |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
Linear Mold Shrinkage, Transverse | 0.0016 cm/cm | 0.0016 in/in | ISO 294-4, 2577 |
Lanxess Durethan® DP A 32 901510 Nylon 66 PA 66 standard injection molding grade, non-reinforced, very easy release |
|||
Linear Mold Shrinkage, Transverse | 0.0016 cm/cm | 0.0016 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® BKV 15 DUS008 000000 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0016 cm/cm | 0.0016 in/in | Eurotec |
Eurotec® Tecodur® PB70 NL TD20 PBT, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.0016 cm/cm | 0.0016 in/in | ISO 294-4, 2577 |
Lanxess Pocan® B 700 000000 PBT