Kinematic Viscosity 56 cSt

@Temperature 140 °C
56 cSt

@Temperature 284 °F
ASTM D445
ExxonMobil SpectraSyn Ultra™ 150 High VI Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn Ultra™ High VI Polyalphaolefin (PAO) have high viscosity indices, low pour points, low traction, good air release, and low foaming tendency. The extremely high visco..