Polymer Property : Kinematic Viscosity = 3.92 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity 3.92 cSt

@Temperature 260 °C
3.92 cSt

@Temperature 500 °F
Duratherm S Silicone Heat Transfer Fluid
Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s..