Kinematic Viscosity 27.5 cSt

@Temperature 50.0 °C
27.5 cSt

@Temperature 122 °F
ChevronTexaco Texatherm®
Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging ..