Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 0.64 cSt @Temperature 0.000 °C |
0.64 cSt @Temperature 32.0 °F |
|
Solvay Specialty Polymers Galden® HT55 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |