Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 0.46 cSt @Temperature 125 °C |
0.46 cSt @Temperature 257 °F |
|
Solvay Specialty Polymers Galden® D02TS PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |