Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 9900 cP @Shear Rate 11200 1/s, Temperature 200 °C |
9900 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE) Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat .. |