Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 97000 cP @Shear Rate 5000 1/s, Temperature 200 °C |
97000 cP @Shear Rate 5000 1/s, Temperature 392 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |