Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 91.9 cP @Temperature 40.0 °C |
91.9 cP @Temperature 104 °F |
|
Teknor Apex TruVis Esters™ TNTM TriNonyl Trimellitate |