Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 90990 cP @Shear Rate 5000 1/s, Temperature 260 °C |
90990 cP @Shear Rate 5000 1/s, Temperature 500 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers |