Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 900000 cP @Shear Rate 1.00 1/s, Temperature 40.0 °C |
900000 cP @Shear Rate 1.00 1/s, Temperature 104 °F |
cone/plate |
Dow BETAMATE™ 1045 Epoxy BETAMATE™ 1045 is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excellent.. |