Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 80000 - 90000 cP @Temperature 25.0 °C |
80000 - 90000 cP @Temperature 77.0 °F |
Part A; 0.50mm Gap, 40mm Parallel Plate, Strain = 0.01%; Bohlin Rheometer |
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and .. |