Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 86190 cP @Shear Rate 5000 1/s, Temperature 285 °C |
86190 cP @Shear Rate 5000 1/s, Temperature 545 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66
(Unverified Data**) 43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |