Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 86.5 cP @Temperature 40.0 °C |
86.5 cP @Temperature 104 °F |
|
Teknor Apex TruVis Esters™ TOTM TriOctyl Trimellitate |