Polymer Property : Viscosity = 85140 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 85140 cP

@Shear Rate 5000 1/s,
Temperature 260 °C
85140 cP

@Shear Rate 5000 1/s,
Temperature 500 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK692FR BK507 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by ..
Viscosity 85140 cP

@Shear Rate 5000 1/s,
Temperature 260 °C
85140 cP

@Shear Rate 5000 1/s,
Temperature 500 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK692FR NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by ..