Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 84630 cP @Shear Rate 5000 1/s, Temperature 205 °C |
84630 cP @Shear Rate 5000 1/s, Temperature 401 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b.. |