Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 84480 cP @Shear Rate 5000 1/s, Temperature 270 °C |
84480 cP @Shear Rate 5000 1/s, Temperature 518 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |