Polymer Property : Viscosity = 81230 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 81230 cP

@Shear Rate 5000 1/s,
Temperature 245 °C
81230 cP

@Shear Rate 5000 1/s,
Temperature 473 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6  (Unverified Data**)
Toughened Polyamide 6Information provided by DuPont Performance Polymers