Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 79440 cP @Shear Rate 5000 1/s, Temperature 280 °C |
79440 cP @Shear Rate 5000 1/s, Temperature 536 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc.. |