Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 79000 cP @Shear Rate 300 1/s, Temperature 190 °C |
79000 cP @Shear Rate 300 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2553 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and impact strength with excellent stiffness for hou.. |