Physical Properties Metric English Comments
Viscosity 77960 cP

@Shear Rate 5000 1/s,
Temperature 230 °C
77960 cP

@Shear Rate 5000 1/s,
Temperature 446 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers