Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 77790 cP

@Shear Rate 5000 1/s,
Temperature 260 °C
77790 cP

@Shear Rate 5000 1/s,
Temperature 500 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&l
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with su..